Titanium End Cap Introduction

Titanium end cap has a series of advantages, such as excellent corrosion resistance, small density, high specific strength, good toughness and weldability. It has been successfully applied in aerospace, petrochemical, shipbuilding, medical, automotive, marine engineering and other fields.
1.Details of titanium end cap
|
Standard |
ASTM B381 |
|
performance |
Titanium forgings have high strength and small density, good mechanical properties, good toughness and corrosion resistance |
|
Status |
Annealed state (M) Thermal processing state (R) (annealed, supersonic flaw detection) |
|
Features |
1. Excellent resistance to corrosive and erosive action of high-temperature acid steam and brine, 2. High strength 3. High resistance to pitting, crevice corrosion resistance 4. High strength to weight ratio 5.Weight saving possibilities 6. Low modulus, high fracture toughness and fatigue resistance 7. Suitability for coiling and laying on seabed 8.Ability to withstand hot/dry and cold/wet acid gas loading |
|
Product Description |
Diameter customizable Technique Hot Forging Surface Smooth surface processing |
|
Application
|
industry, electronics, medical, chemical, petroleum, pharmaceutical, aerospace, etc. |
2. Chemical composition of titanium end cap
|
Grade |
N |
C |
H |
Fe |
O |
Al |
V |
Pd |
Mo |
Ni |
Ti |
|
Gr1 |
0.03 |
0.08 |
0.015 |
0.20 |
0.18 |
/ |
/ |
/ |
/ |
/ |
Balance |
|
Gr2 |
0.03 |
0.08 |
0.015 |
0.30 |
0.25 |
/ |
/ |
/ |
/ |
/ |
Balance |
|
Gr5 |
0.05 |
0.08 |
0.015 |
0.40 |
0.20 |
5.5-6.75 |
3.5- 4.5 |
/ |
/ |
/ |
Balance |
|
Gr7 |
0.03 |
0.08 |
0.015 |
0.30 |
0.25 |
/ |
/ |
0.12-0.25 |
/ |
/ |
Balance |
|
Gr9 |
0.03 |
0.08 |
0.015 |
0.25 |
0.15 |
2.5- 3.5 |
2.0- 3.0 |
/ |
/ |
/ |
Balance |
|
Gr12 |
0.03 |
0.08 |
0.015 |
0.30 |
0.25 |
/ |
/ |
/ |
0.2-0.4 |
0.6-0.9 |
Balance |
|
Gr23 |
0.03 |
0.08 |
0.012 |
0.25 |
0.13 |
5.5-6.5 |
3.5-4.5 |
/ |
/ |
/ |
Balance |
3.Mechanical properties of titanium end cap
|
Grade |
Tensile Strength, Min MPa |
Yield Strength Min MPa |
Elongation in 4D,Min, % |
Reduction of Area,min % |
|
Gr1 |
240 |
138 |
24 |
30 |
|
Gr2 |
345 |
275 |
20 |
30 |
|
Gr3 |
450 |
380 |
18 |
30 |
|
Gr4 |
550 |
483 |
15 |
25 |
|
Gr5 |
895 |
828 |
10 |
25 |
|
Gr7 |
345 |
275 |
20 |
30 |
|
Gr9 |
620 |
483 |
15 |
25 |
|
Gr12 |
483 |
345 |
18 |
25 |
|
Gr16 |
345 |
275 |
20 |
30 |
|
Gr23 |
828 |
759 |
10 |
15 |
4.Specification of titanium end cap
|
Product Name |
Dimensions |
Grade |
Standards |
||
|
Outer Diameter |
Inner Diameter |
Height |
|||
|
Disc |
50~200 |
/ |
20~140 |
GR1,GR2,GR5,GR7, GR9, GR12,GR23 |
ASTM B381 |
|
200~400 |
/ |
25~150 |
|||
|
400~600 |
/ |
30~110 |
|||
|
Ring |
200~400 |
100~300 |
20~150 |
||
|
400~700 |
150~500 |
30~250 |
|||
|
700~900 |
300~700 |
35~300 |
|||
|
900~1300 |
400~900 |
50~400 |
5.Defects of titanium alloy forgings
a.Segregation type defect
In addition to β segregation, β spot, titanium rich segregation and strip α segregation, the most dangerous is the interstitial α stable segregation (I-type α segregation), which is often accompanied by small holes and cracks, containing oxygen, nitrogen and other gases, and is brittle. There are also aluminum rich α stable segregation (type II α segregation), which also has dangerous defects due to cracks and brittleness, and will reduce the thermal stability and other properties of the alloy.
b. inclusions
There are inclusions on the surface of the blank, and cracks often form along the inclusions during forging, or obvious foreign objects appear after corrosion of the forging, most of which are high melting point and high-density metal inclusions. The high melting point and high-density elements in titanium alloys have not completely melted and remain in the matrix (such as molybdenum inclusions)
c. holes
The holes may not exist alone, but may also exist in a number of dense, which will speed up the low cycle fatigue crack growth and lead to early fatigue failure.
d. crack
It mainly refers to forging cracks. Titanium alloy has large viscosity, poor fluidity, and poor thermal conductivity. Therefore, in the process of forging deformation, due to large surface friction, obvious internal deformation nonuniformity and large temperature difference between the inside and outside, it is easy to produce shear bands (strain lines) inside the forging. In serious cases, cracks occur along the direction of maximum deformation stress.
e. overheating
Titanium alloy has poor thermal conductivity. In addition to overheating of forgings or raw materials due to improper heating during hot working, it is also easy to overheat due to thermal effect during deformation during forging, resulting in microstructure change and overheating of Widmanstatten structure.

In order to ensure the quality of titanium alloy forgings, in addition to strictly controlling the quality of raw materials, we should also pay attention to the ultrasonic testing of the forging blanks and semi-finished products to prevent some deformation and physical properties of the defects that will change in the subsequent heating process.
6.FAQ
FAQ

01.Are You Trading Company Or Manufacturer ?
02.How Long Is Your Delivery Time?
03.Do You Provide Samples ? Is It Free Or Extra ?
04.What's the payment term ?
Hot Tags: titanium end cap, China titanium end cap manufacturers, suppliers, factory, 381 Titanium Disk, Titanium Flange, Gr5 Titanium Block, 381 Titanium Block, Titanium Machining Parts, Titanium End Cap